Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.221 GPa | 32.1 ksi | ISO 178/1A |
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | 2% Secant; ASTM D 790 |
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding
(discontinued **) Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 1.. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 1810A Polyethylene
(discontinued **) Polyethylene 1810A contains no additives. It is suggested for injection molding applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to West.. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 1810E Polyethylene
(discontinued **) Polyethylene 1810E contains no additives. It is suggested for general purpose extrusion applications requiring good stress crack resistance or electrical properties. It is used in applications suc.. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 18DOA Polyethylene
(discontinued **) Polyethylene 18DOA is a low density formulation suggested for the production of closures where a high melt index material is needed to meet shrinkage requirements and fast molding cycles. It molds .. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | ASTM D790 |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Flexural Modulus | 0.221 GPa | 32.1 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 1122B Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati.. |