Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific) |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | Injection molded; ASTM D790 |
Americas Styrenics STYRON™ A-TECH™ 6079 Ignition Resistant Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 6079 is an ignition resistant polystyrene (IRPS) resin designed specifically for consumer and business electronics applications that demand excellent aesthetics, along with a stron.. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL INT2001 PPE+HIPS (Asia Pacific) PPE+PS Unfilled for Auto Interior |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.09 GPa @Temperature 260 °C |
303 ksi @Temperature 500 °F |
ASTM D790 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® X0718 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2630 PPE+HIPS (Asia Pacific) PPE+HIPS Unfilled high Impact |
|||
Flexural Modulus | 2.09 GPa | 303 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated. |