Mechanical Properties Metric English Comments
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced
Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
Flexural Modulus 3.93 GPa
570 ksi
1.3 mm/min; ASTM D790
PolyOne Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 3.93 GPa
570 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics REMEX VR4831 PBT
15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite..
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Techmer ES Electrablend® PC 04009 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite..
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Techmer ES HiFill® ABS WM20 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p..
Flexural Modulus 3.93 GPa
570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP
LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized.
Flexural Modulus 3.93 GPa
570 ksi
Tangent; ASTM D790
Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar..
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Asahi Kasei Thermylene® P6-23FG-2600 23% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS
Information provided by Asahi Thermofil
Flexural Modulus 3.93 GPa
570 ksi
ASTM D790
PlastxWorld CEVIAN® A2604 20% GF PA/ABS Alloy, Conditioned
Property data is for samples at equilibrium moisture (1.1%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo..