Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech ABS ABS833G10L Glass Reinforced |
|||
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G5M25CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336M30CL Mica Reinforced Coupled |
|||
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339G5M25CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech Nylon 6 NY0730G10L Glass Reinforced |
|||
Flexural Modulus | 3.900 GPa | 565.6 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G25M5CL Glass/Mineral Reinforced Coupled |