Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.73 GPa @Thickness 3.20 mm |
540 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.73 GPa @Thickness 3.20 mm |
540 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 120PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 121PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 129PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP, ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 320PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa @Temperature 23.0 °C |
540 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 540 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.73 GPa | 541 ksi | ASTM D790 |
LNP ULTEM® JD7904 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |