Mechanical Properties Metric English Comments
Flexural Modulus 3.13 GPa
454 ksi
ASTM D638
Network Polymers MS 200 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1005 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East)
High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/..
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Asia Pacific)
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin.
Flexural Modulus 3.13 GPa
454 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics EXTEM XH1015F TPI Resin (Europe-Africa-Middle East)
Thermoplastic Polyimide Extem* XH1015 Resin. EFSA food Contact approved.
Flexural Modulus 3.13 GPa
454 ksi
ASTM D790
PolyOne Stat-Tech™ NN-20SS/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 3.13 GPa

@Temperature 23.0 °C
454 ksi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT™ 2062 Polyimide, Anthrazit Gleamy, 15% Graphite, 10% PTFE (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...