Mechanical Properties Metric English Comments
Flexural Modulus 3.02 GPa
438 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers MS 110 Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Flexural Modulus 3.02 GPa
438 ksi
ASTM D790
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Flexural Modulus 3.02 GPa
438 ksi
ASTM D790
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 3.02 GPa
438 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP COLORCOMP EX10304C PEI (Asia Pacific)
LNP* Colorcomp* EX10304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS Technol..
Flexural Modulus 3.02 GPa
438 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.02 GPa
438 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.02 GPa
438 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.02 GPa
438 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12
LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
Flexural Modulus 3.02 GPa
438 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Flexural Modulus 3.02 GPa
438 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
Flexural Modulus 3.02 GPa
438 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific)
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
Flexural Modulus 3.02 GPa
438 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an..
Flexural Modulus 3.02 GPa
438 ksi
ISO 178-93
Wellman Wellamid® 22L-BL Engineering Grade Nylon 66
Description: Engineering Grade Nylon 66Information provided by Wellman.
Flexural Modulus 3.02 GPa
438 ksi
ASTM D-790
Axiall 7765 Rigid PVC, Extrusion
Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo..
Flexural Modulus 3.02 GPa
438 ksi
ASTM D790
Ineos Nova 3510 General Purpose Crystal Polystyrene  (discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..
Flexural Modulus 3.02 GPa
438 ksi
ASTM D790
Ineos Nova 3511 General Purpose Crystal Polystyrene  (discontinued **)
Excellent blending resin, Suitable fore difficult to fill and thin wall molding, USP Class VIApplications: Single service cutlery, Cosmetic and medical molding, Consumer electronic packagingExposure..