Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.400 - 3.00 GPa | 58.0 - 435 ksi | Average value: 2.19 GPa Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 0.696 - 3.00 GPa | 101 - 435 ksi | Average value: 1.50 GPa Grade Count:41 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 0.814 - 3.00 GPa | 118 - 435 ksi | Average value: 1.84 GPa Grade Count:43 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Flexural Modulus | 2.50 - 3.00 GPa | 363 - 435 ksi | ASTM D790 |
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Flexural Modulus | 2.70 - 3.00 GPa | 392 - 435 ksi | ASTM D790 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Flexural Modulus | 2.00 - 3.00 GPa | 290 - 435 ksi | ASTM D790 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Modulus | 2.70 - 3.00 GPa | 392 - 435 ksi | ASTM D790 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |
|||
Flexural Modulus | 0.700 - 3.00 GPa | 102 - 435 ksi | Average value: 1.45 GPa Grade Count:42 |
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |