Mechanical Properties Metric English Comments
Flexural Modulus 1.92 GPa
278 ksi
13 mm/min; ASTM D790
PolyOne Geon™ L4605 Ivory 3098 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid)
Information provided by PolyOne
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare.
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO
LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON WS002I PBT
LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact.
Flexural Modulus 1.92 GPa
278 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific)
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead.
Flexural Modulus 1.92 GPa
278 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead.
Flexural Modulus 1.92 GPa
278 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Flexural Modulus 1.92 GPa
278 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.92 GPa
278 ksi
ASTM D790
Teknor Apex Sinpolene CPP1030 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F..
Flexural Modulus 1.92 GPa
278 ksi
At 2 mm/min; ISO 527-2
Borealis Daplen™ ED206HP TPO Compound
Daplen ED206HP is a 25% mineral reinforced compound intended for injection molding. ED206HP has been developed especially for the car industry, to be used in interior parts requiring excellent scra..
Flexural Modulus 1.92 GPa
278 ksi
ISO R178
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Flexural Modulus 1.92 GPa
278 ksi
23°C, 50% RH; ASTM D790
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Flexural Modulus 1.92 GPa
278 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRILOY Z20001 PPO
LNP* Lubriloy* Z20001 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.