Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2760 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 16.0 - 19.0 GPa
2320 - 2760 ksi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel..
Flexural Modulus 16.0 - 19.0 GPa
2320 - 2760 ksi
Injection; ISO 178
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Flexural Modulus 11.7 - 19.0 GPa
1700 - 2760 ksi
Average value: 14.6 GPa Grade Count:12
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Flexural Modulus 7.53 - 19.0 GPa
1090 - 2760 ksi
Average value: 11.5 GPa Grade Count:3
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 6.70 - 19.0 GPa
972 - 2760 ksi
Average value: 8.15 GPa Grade Count:19
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum ..
Flexural Modulus 7.20 - 19.0 GPa

@Temperature -40.0 - 80.0 °C
1040 - 2760 ksi

@Temperature -40.0 - 176 °F
Average value: 13.4 GPa Grade Count:1
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Flexural Modulus 14.0 - 19.0 GPa
2030 - 2760 ksi
ISO 178
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
Copyright © lookpolymers.com All Rights Reserved