Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Multibase Multi-Pro® 3014 CUW Polypropylene Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Nylene® 8100 Unfilled Nylon 6/12 Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/ABS Alloy Polycarbonate/ABS AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Network Polymers 351 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM 408 L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | secant; ASTM D790 |
Spartech PP5120 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Teknor Apex Synres® SR 1288A Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | 1% Secant; ASTM D790 |
Washington Penn Homopolymer Polypropylene 20% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | Tangent; ASTM D790 |
Washington Penn Medium Impact Copolymer 40% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7600B (ELG) Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Ensinger Tecamid® 6/12 Nylon (PA612) Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Clariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Adell ZS-10 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Adell ZS-30 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
Americas Styrenics STYRON® 484 High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation pr.. |
|||
Flexural Modulus | 1.90 GPa | 275 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |