Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 273 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.88 GPa
273 ksi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 1.88 GPa
273 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.88 GPa
273 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
Flexural Modulus 1.88 GPa
273 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 1.88 GPa
273 ksi
ASTM D790
Metton LMR M1534 Liquid Molding Resin
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce ..
Flexural Modulus 1.88 GPa
273 ksi
Kraton® G1654 + PPE blend (20/80)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PPE significantly improves the..
Flexural Modulus 1.88 GPa
273 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS
LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release.
Flexural Modulus 1.88 GPa
273 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S190
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 1.88 GPa
273 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S750
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 1.88 GPa
273 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 1.88 GPa
273 ksi
parallel; ASTM D790
Dow SPECTRIM™ HH 390 Reaction Moldable Polymer
Information provided by Dow
Flexural Modulus 1.88 GPa
273 ksi
ASTM D790
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Flexural Modulus 1.88 - 11.4 GPa
273 - 1650 ksi
Average value: 4.43 GPa Grade Count:104
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..