Polymer Property : Flexural Modulus = 271 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.87 GPa
271 ksi
ASTM D790
PolyOne Nymax™ 2024 HS UV 425C Grey Polyamide 66 (Nylon 66)
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o..
Flexural Modulus 1.87 GPa
271 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
Flexural Modulus 1.87 GPa
271 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12
LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 1.87 GPa
271 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V2105U PBT
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
Flexural Modulus 1.87 GPa
271 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East)
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.
Flexural Modulus 1.87 GPa

@Thickness 19.0 mm
271 ksi

@Thickness 0.750 in
ASTM D790
3A Composites Core Materials AIREX® PXw.320 Fiber-Reinforced Structural Foam Panel
AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou..
Flexural Modulus 1.87 GPa
271 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific)
Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio.