Polymer Property : Flexural Modulus = 27.6 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
Quantum Composites HTC-9500 55% E-Glass Fiber Reinforced Bismaleimide SMC, High Temperature Composite
HTC-9500 (127-51-6) is an E-Glass Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics providing ..
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4182 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance..
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding
Information provided by PolyOne™ Corporation
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Flexural Modulus 27.6 GPa
4000 ksi
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Flexural Modulus 27.6 GPa
4000 ksi
Carlisle 201HD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Flexural Modulus 27.6 GPa
4000 ksi
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Flexural Modulus 27.6 GPa
4000 ksi
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Flexural Modulus 27.6 GPa
4000 ksi
Carlisle 201LD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..