Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.186 GPa | 27.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips KN 226B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; Mold Release Agent Added; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Excellent Mold Release, Mode.. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips 1400 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C.. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips 4538B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso.. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | ASTM D790 |
ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer resin designed for electrical applications.Applications: Base resin for medium voltage power cable insulati.. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | ASTM D790 |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | 3 pt. secant; ASTM D790 |
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 22200Characteristics: Good Flexibility, Excellent Flow, Good Warping Resistance, Good Mold Release, Moderate ESCRApplications:Houseware.. |
|||
Flexural Modulus | 0.186 GPa | 27.0 ksi | ASTM D790 |
Multibase Multi-Flam™ 0803 LDPE NH Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |