Mechanical Properties Metric English Comments
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific)
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton UV00A PPA
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton UV00A PPA (Asia Pacific)
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Verton UV00ASXS PPA (Europe-Africa-Middle East)
LNP* VERTON* UV00ASXS is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA
LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural.
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ASTM D790
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Flexural Modulus 17.7 GPa
2570 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific)
VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass.
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
LNP Verton™ UF-700-10 Polyphthalamide, Long Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Flexural Modulus 17.7 GPa
2570 ksi
ISO 178
SABIC Innovative Plastics LNP Verton OX07411 PPS
LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.