Mechanical Properties Metric English Comments
Flexural Modulus 1.758 GPa
255.0 ksi
ASTM D790
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.758 GPa
255.0 ksi
ASTM D790
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp
Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c..
Copyright © lookpolymers.com All Rights Reserved