Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.75 GPa | 254 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | Chord; 2 mm/min; ISO 178 |
Mytex Polymers AS88LW-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol H050MN Polypropylene REPOL Polypropylene H050MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 1% secant; ASTM D790A |
Reliance Industries Repol H110MS Polypropylene REPOL Polypropylene H110MS is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ASTM D790 |
I. Stern 870E High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetprofilesAgency Rating.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-C111 Toughened PA66 Features:High impactLow tendency to wrapExcellent balance propertiesApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0242 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ASTM D790 |
Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene HIPS7240 is a very high impact polystyrene used in the extrusion industry. The good melt strength of this grade makes it particularly suitable for deep-draw thermoforming. HIPS 7240 is available in .. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO Data |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 2mm/min; ISO 178 |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | 2mm/min; ISO 178 |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178-93 |
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy Description: Nylon/Polypropylene AlloyInformation provided by Wellman. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ASTM-D790 |
Polyram RamTal PM1409 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | dry; ISO 178 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | SAE J949 |
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ASTM D790 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO Data |
BASF Ultramid® 8350 HS PA6 (Dry) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
A.D. Compound Adene NTFAG Copolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Flexural Modulus | 1.75 GPa | 254 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP2040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |