Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.80 - 25.0 GPa @Temperature -40.0 - 250 °C |
406 - 3630 ksi @Temperature -40.0 - 482 °F |
Average value: 9.10 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Flexural Modulus | 2.80 - 25.0 GPa @Thickness 0.800 - 3.17 mm |
406 - 3630 ksi @Thickness 0.0315 - 0.125 in |
Average value: 9.10 GPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |