Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 24.1 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 24.1 GPa
3500 ksi
0°; measured on 0.1" panel molded from tape; ASTM D790
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
Flexural Modulus 24.1 GPa

@Temperature 23.9 °C
3500 ksi

@Temperature 75.0 °F
Dry; 325°F Autoclave Cured; ASTM D790
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Flexural Modulus 24.1 GPa
3500 ksi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In..
Flexural Modulus 24.1 GPa
3500 ksi
ASTM D790
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Flexural Modulus 24.1 GPa
3500 ksi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide..
Flexural Modulus 24.1 GPa
3500 ksi
90° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Flexural Modulus 24.1 GPa
3500 ksi
0° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Flexural Modulus 24.1 GPa
3500 ksi
ASTM D790
PolyOne Edgetek® AM-40CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved