Mechanical Properties Metric English Comments
Flexural Modulus 1.49 GPa
216 ksi
Method I (3 point load), Procedure B); ASTM D790
Multibase Nylex™ 2185 HF Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 1.49 GPa
216 ksi
Tangent; ASTM D790
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.49 GPa
216 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790
Network Polymers NPP 30-3500 NA
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 1.49 GPa
216 ksi
Tangent; ASTM D790
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.49 GPa
216 ksi
1% Secant; ASTM D790
Flint Hills P4G3Z-039 Homopolymer Polypropylene
Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills..
Flexural Modulus 1.49 GPa
216 ksi
1% secant; ASTM D790-02
Ipiranga Petrochem PH 2610 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Flexural Modulus 1.49 GPa
216 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON MX01767C PP
LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Flexural Modulus 1.49 GPa
216 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Flexural Modulus 1.49 GPa
216 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS
LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993...
Flexural Modulus 1.49 GPa
216 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..
Flexural Modulus 1.49 GPa
216 ksi
ASTM D790
Total PPH M3382MZ Homopolymer Polypropylene, Clarified Metallocene Sheet Extrusion and Thermoforming Resin
Clarity. TOTAL Polypropylene M3382MZ produces thermoformed parts with superior clarity, gloss and excellent side wall stiffness.Recommended Applications. TOTAL Polypropylene M3382MZ is ideal for d..
Flexural Modulus 1.49 GPa
216 ksi
Cyclewood Solutions Xylomer™ XM2-CUA Sustainable Injection Molding Resin
100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural bypro..
Flexural Modulus 1.49 GPa
216 ksi
ASTM D790
Braskem H 107 Injection Molding Polypropylene
Applications: Thin-walled parts and easy mould filling. Information provided by Braskem
Flexural Modulus 1.49 GPa
216 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..