Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.8 GPa | 2150 ksi | |
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre FeaturesChemically reinforced with 40% carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. .. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Flexural Modulus | 14.8 GPa @Temperature 150 °C |
2150 ksi @Temperature 302 °F |
ASTM D790 |
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF00AAS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF00AAS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ISO 178-93 |
Wellman Wellamid® GF1750-BK2 50% Glass Fiber Reinforced Nylon 6 Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ASTM D790 |
Plenco 6401 Phenolic, Briquette, Injection Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Flexural Modulus | 14.8 - 33.1 GPa | 2150 - 4800 ksi | Average value: 22.9 GPa Grade Count:12 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Flexural Modulus | 14.8 GPa | 2150 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |