Mechanical Properties Metric English Comments
Flexural Modulus 1.379 GPa
200.1 ksi
ASTM D790
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.379 GPa
200.1 ksi
ASTM D790
Lucent Polymers PPH-110 Polypropylene, Homopolymer
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.379 GPa
200.1 ksi
ASTM D790
Lucent Polymers TPP-210 Polypropylene, 10% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.