Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 20.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 17.0 - 20.0 GPa
2470 - 2900 ksi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Flexural Modulus 15.0 - 20.0 GPa
2180 - 2900 ksi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
Flexural Modulus 16.0 - 20.0 GPa
2320 - 2900 ksi
Compression; ISO 178
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Flexural Modulus 1.57 - 20.0 GPa
228 - 2900 ksi
Average value: 2.34 GPa Grade Count:134
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Flexural Modulus 6.60 - 20.0 GPa
957 - 2900 ksi
Average value: 11.5 GPa Grade Count:24
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Flexural Modulus 4.00 - 20.0 GPa
580 - 2900 ksi
Average value: 9.89 GPa Grade Count:37
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Flexural Modulus 3.00 - 20.0 GPa
435 - 2900 ksi
Average value: 10.1 GPa Grade Count:21
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Modulus 10.0 - 20.0 GPa
1450 - 2900 ksi
Parallel to Plane
Goodfellow Carbon-Carbon Composite
Carbon Fiber - Carbon MatrixInformation provided by Goodfellow.
Flexural Modulus 0.469 - 20.0 GPa
68.0 - 2900 ksi
Average value: 4.97 GPa Grade Count:236
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Flexural Modulus 15.0 - 20.0 GPa
2180 - 2900 ksi
Compression; ISO 178
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
Copyright © lookpolymers.com All Rights Reserved