Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.78 GPa | 403 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | ISO 178 |
Polyplastics Duranex® 209A Polybutylene Terephthalate (PBT), Low friction, Low wear DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 2.78 GPa | 403 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |