Polymer Property : Flexural Modulus = 2.52 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.52 GPa
365 ksi
Method I (3 point load), Procedure B); ASTM D790
Multibase Nylex™ 2185 R20 Natural Polyamide + PP
Forms: PelletsInformation provided by Multibase
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L9620 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Flexural Modulus 2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications.
Flexural Modulus 2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications.
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Ravago Manufacturing Americas Hylac® PL75 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 2.52 GPa
365 ksi
Tangent; ASTM D790
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Global ABS-1805 General Purpose ABS  (discontinued **)
Information provided by Global Polymers Corporation.
Flexural Modulus 2.52 GPa
365 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS
LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO
LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.52 GPa
365 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC
LNP* STAT-KON* D-FR is a compound based on Polycarbonate resin containing Carbon. Added features of this grade include: Flame Retardant, Electrically Conductive.
Flexural Modulus 2.52 GPa
365 ksi
tangent; ASTM D790
Spartech PP7130 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Techmer ES Plastiblend® PC/PBT IM 1702 BK
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Modulus 2.52 GPa
365 ksi
ISO 178
SABIC Innovative Plastics NORYL N300X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Modulus 2.52 GPa
365 ksi
ISO 178
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Modulus 2.52 GPa
365 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL NH7010 PPE+PS
Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts..
Flexural Modulus 2.52 GPa
365 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific)
High heat, Non halogenated flame retardant Noryl product
Flexural Modulus 2.52 GPa
365 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Flexural Modulus 2.52 GPa
365 ksi
Tangent; ASTM D790
Plastics Group Polifil® RMT-30 30% Talc-Reinforced Polypropylene, High Impact
Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis..
Flexural Modulus 2.52 GPa
366 ksi
Procedure B, Test Method I(chs 0.05 in/min); ASTM D790
Diamond Polymers ABS TX-541
Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc.