Polymer Property : Flexural Modulus = 2.32 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.32 GPa
337 ksi
Tangent (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 808 C5WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Flexural Modulus 2.32 GPa
336 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers PC-1030L
Description: Polycarbonate Information provided by Network Polymers Inc.
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific)
Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Asia Pacific)
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl..
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer
High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Asia Pacific)
High visocisty PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East)
High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP COLORCOMP D10006U PC
LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed.
Flexural Modulus 2.32 GPa
336 ksi
ASTM D790
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin  (discontinued **)
Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o..
Flexural Modulus 2.32 GPa
336 ksi
ASTM D790
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet
KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an..
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp DP0039 PC
LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP QL004 PA6.10
LNP* LUBRICOMP* QL004 is a compound based on Nylon 6/10 containing 20% PTFE. Added features of this grade include: Wear Resistant.
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER
F-1 weathering certified in natural color, specially designed for Pool & Spa applications.
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
Flexural Modulus 2.32 GPa
336 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF)
LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.32 GPa
337 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.32 GPa
337 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Flexural Modulus 2.32 GPa
336 ksi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy
Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed..
Flexural Modulus 2.32 GPa
336 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 3500 Natural 1050
Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.32 GPa
336 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 4500R
Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.32 GPa
336 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 4502
Description: Injection Molding Grade, Medium Impact Information provided by Diamond Polymers, Inc.
Flexural Modulus 2.32 GPa
336 ksi
ASTM D790
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the..
Flexural Modulus 2.32 GPa
336 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East)
High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.