Mechanical Properties Metric English Comments
Flexural Modulus 0.0150 GPa
2.18 ksi
ISO 178
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding
Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend..
Flexural Modulus 0.0150 GPa
2.18 ksi
BS4370, part 4, method 14
Zotefoams Plastazote® HD80 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Flexural Modulus 0.0150 GPa
2.18 ksi
ASTM D790
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Flexural Modulus 0.0150 GPa
2.18 ksi
ASTM D790
Toyobo Pelprene™ P-30B Polyester TPE
Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block..
Flexural Modulus 0.0150 - 3.09 GPa
2.18 - 448 ksi
Average value: 0.408 GPa Grade Count:63
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..