Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 199.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.373 GPa
199.1 ksi
ASTM D790
LG Chemical HI835HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Flexural Modulus 1.373 GPa
199.1 ksi
ASTM D790
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Copyright © lookpolymers.com All Rights Reserved