Polymer Property : Flexural Modulus = 1983 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 13.67 GPa
1983 ksi
ASTM D 790
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 13.67 GPa
1983 ksi
ASTM D 790
SABIC Innovative Plastics LNP Verton RX93407D PA 66 (Asia Pacific)
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Asia Pacific region.