Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.9 GPa | 2890 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data .. |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized. |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | ASTM D790 |
Plenco 1510 Polyester, Granular, Transfer Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Flexural Modulus | 19.9 GPa | 2890 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |