Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific) LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/40 Polycarbonate, 40% Carbon Fiber Reinforced, PTFE Lubricated |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF60 TL10 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 8575101Information provi.. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific) LNP* Thermocomp* UFW49S is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ASTM D790 |
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 19.3 GPa | 2800 ksi | ISO 178 |
LNP Thermocomp® UFM-3249 HS BK8-115 Polyphthalamide, Glass Mineral Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |