Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.1 GPa | 2770 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Flexural Modulus | 19.1 GPa | 2770 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 19.1 GPa | 2770 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6 LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 19.1 GPa | 2770 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Flexural Modulus | 19.1 GPa | 2770 ksi | ASTM D790 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |