Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.1946 GPa @Thickness 3.20 mm |
173.27 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |