Mechanical Properties Metric English Comments
Flexural Modulus 1.175 GPa
170.4 ksi
12.5 mm/min; ASTM D790
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade
ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys..
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.
Flexural Modulus 1.175 GPa
170.4 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 401 Ionomer
Information provided by A. Schulman.