Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.56 GPa | 1677 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 11.56 GPa | 1677 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF008 PC LNP THERMOCOMP* DF008 is a compound based on Polycarbonate resin containing 40% Glass Fiber. |