Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.8 GPa | 2440 ksi | ASTM D790 |
PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 16.8 GPa | 2440 ksi | ASTM D790 |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 16.8 GPa | 2440 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Flexural Modulus | 16.8 GPa @Temperature 100 °C |
2440 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Flexural Modulus | 16.8 GPa | 2440 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 16.8 GPa | 2440 ksi | ISO 178 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Flexural Modulus | 16.8 GPa @Temperature 100 °C |
2440 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |