Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
PolyOne OnForce™ LFT NN-60LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 16.0 - 20.0 GPa | 2320 - 2900 ksi | Compression; ISO 178 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Resinoid 1370 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 7/CF/30/BK Polyamide 610, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific) Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V8090 PBT+PET (Europe-Africa-Middle East) 50% Glass Fiber Reinforced PBT-PET resin |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 16.0 - 18.0 GPa | 2320 - 2610 ksi | Compression; ISO 178 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Resinoid 1320 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 16.0 - 18.0 GPa | 2320 - 2610 ksi | Injection; ISO 178 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information .. |