Polymer Property : Flexural Modulus = 1545 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.65 GPa
1545 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410EPR PEI
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Flexural Modulus 10.65 GPa
1545 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Flexural Modulus 10.65 GPa
1545 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing.
Flexural Modulus 10.65 GPa
1545 ksi
ISO 178
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66
LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ..