Mechanical Properties Metric English Comments
Flexural Modulus 10.30 GPa
1494 ksi
ASTM D790
E-Polymers SEPAZ® V330HS 30% Glass Fiber Reinforced Heat Stabilized PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Flexural Modulus 10.30 GPa
1494 ksi
ASTM D790
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Flexural Modulus 10.30 GPa
1494 ksi
ASTM D790
E-Polymers SEPAZ® V230A 30% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..