Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 14.32 GPa | 2077 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EE005 PEI LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Flexural Modulus | 14.32 GPa | 2077 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific) LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the .. |
|||
Flexural Modulus | 14.32 GPa | 2077 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Flexural Modulus | 14.32 GPa | 2077 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific) LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 14.32 GPa | 2077 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific) LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |