Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.580 - 0.830 GPa | 84.1 - 120 ksi | Average value: 0.760 GPa Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Carbon Black Filled". Each property range of values reported is minimu.. |
|||
Flexural Modulus | 0.621 - 0.827 GPa | 90.0 - 120 ksi | ASTM D790 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.621 - 0.827 GPa | 90.0 - 120 ksi | ASTM D790 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Flexural Modulus | 0.00383 - 0.830 GPa | 0.555 - 120 ksi | Average value: 0.124 GPa Grade Count:19 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Flexural Modulus | 0.620 - 0.827 GPa | 89.9 - 120 ksi | ASTM D790 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |