Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 12.7 GPa | 1840 ksi | |
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Modulus | 12.7 GPa @Temperature 23.0 °C |
1840 ksi @Temperature 73.4 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 12.7 GPa @Thickness 3.20 mm |
1850 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 5 mm/min; ISO 178 |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East) LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON ZE004 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON ZE004 PPO LNP* STAT-KON* ZE004 is a compound based on PPO resin containing 20% Carbon Fiber. Added feature of this grade includes: Electrically Conductive. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | |
Shinil Chemical SHINCON PEI-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ASTM D790 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Flexural Modulus | 12.7 GPa | 1840 ksi | ASTM Test |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G8-43GF Nylon 66, 43% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 12.7 GPa | 1850 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® XP-2140C PPS Information provided by Samsung Cheil Industries. |