Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0848 GPa | 12.3 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 8699 BLK Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by.. |
|||
Flexural Modulus | 0.0850 GPa | 12.3 ksi | ASTM D790 |
LATI LASTANE 50 High Impact Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Flexural Modulus | 0.0850 GPa | 12.3 ksi | ASTM D638 |
Arkema Group LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate LOTRYL® 7 BA 01 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 7 BA 01 is used for film coextrusion and lamination where sealab.. |
|||
Flexural Modulus | 0.0850 GPa | 12.3 ksi | ASTM D638 |
Arkema Group LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate LOTADER AX 8840 is a random copolymer of Ethylene and Glycidyl Methacrylate, polymerized under high pressure in an autoclave process. Due to the reactivity induced by the Glycidyl methacrylate, LOTA.. |