Mechanical Properties Metric English Comments
Flexural Modulus 7.350 GPa
1066 ksi
ASTM D570
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Flexural Modulus 7.350 GPa
1066 ksi
ASTM D570
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).