Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.717 GPa | 104 ksi | 1% Secant; ASTM D790B |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 1.3 mm/min; ASTM D790 |
ICO Polymers ICORENEâ„¢ 155-1339 LMDPE Rotational Molding Resin Description: ICORENE 155-1339 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Flexural Modulus | 0.716 GPa | 104 ksi | |
Kuraray HYBRAR® PP2 Thermoplastic Rubber-Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Asia Pacific) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 12.5 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | ISO 178 |
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® C300 Polyethylene; Enhanced Metallocene medium density polyethylene. This metallocene MDPE resin is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typical blow molded ap.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | 2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Flexural Modulus | 0.720 GPa | 104 ksi | ASTM D790 |
Braskem MR 435 UV LMDPE Rotational Molding Polyethylene Applications: Water tanks; toys; automotive components. Information provided by Braskem |
|||
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |
|||
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E.. |
|||
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R116 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R116 is a thermoplastic polyolefin elastomeric. It is unfilled, reactor-grade molding compound. Applications: Exterior trim Information provided by Solvay Engineered Polymers.. |