Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0715 GPa | 10.4 ksi | ASTM D790 |
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |