Polymer Property : Flexural Modulus = 10.34 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK (Asia Pacific)
LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing Bearing Grade. Added features of this material include: Easy Molding.
Flexural Modulus 10.34 GPa
1500 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6
LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific)
LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret..
Flexural Modulus 10.34 GPa
1500 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Flexural Modulus 10.34 GPa
1500 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features include: Healthcare.
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific)
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber.
Flexural Modulus 10.34 GPa
1500 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RX10409D PA 66
LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural.
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).
Flexural Modulus 10.34 GPa
1500 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA 6/12 (Asia Pacific)
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.