Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0689 GPa | 10.0 ksi | ASTM D790 |
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M.. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0690 GPa | 10.0 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0689 GPa | 10.0 ksi | ASTM D790 |
Lubrizol Estane® ALR E95A Thermoplastic Polyurethane Type: Estane® ALR E95A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
Flexural Modulus | 0.0689 GPa | 10.0 ksi | ASTM D790 |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Flexural Modulus | 0.0689 GPa | 10.0 ksi | ASTM D790 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Flexural Modulus | 0.0689 GPa | 10.0 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Flex® A 8103 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusions Information provided by Multibase |
|||
Flexural Modulus | 0.0689 - 12.8 GPa | 10.0 - 1860 ksi | Average value: 2.39 GPa Grade Count:236 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |