Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |
|||
Flexural Modulus | 1.653 GPa | 239.8 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible.. |